Try the full study dashboard free, no signup: practice, flashcards and your Exam Readiness Score. Open it →
Home / Practice tests / ASNT NDT Level II UT
ASNT · Last updated November 2026

ASNT NDT Level II, Ultrasonic Testing (UT): free practice test

ASNT's third-party written certification for ultrasonic technicians: a 50-item General exam and a 40-item Specific exam for the general industry or pressure equipment sector. Applicants document 120 days of UT experience, 229 days of total NDT experience and 12 days of training. ASNT lists a revised UT General outline for exams after 5 February 2027. This prep covers only the written exams; the visual acuity, practical and any job-specific exams are given by your employer.

Watch the free 4:25 video lesson: the key ASNT NDT Level II UT concepts →

Premium: 3,000 practice questions, 6 full mock exams, 800 flashcards and 60 comprehensive key notes, topic by topic. See the study path ·

Or open the free ASNT NDT Level II UT study dashboard: flashcards, notes and your Readiness Score, no signup →

About the ASNT NDT Level II UT exam

ASNT's third-party written certification for ultrasonic technicians: a 50-item General exam and a 40-item Specific exam for the general industry or pressure equipment sector. Applicants document 120 days of UT experience, 229 days of total NDT experience and 12 days of training. ASNT lists a revised UT General outline for exams after 5 February 2027. This prep covers only the written exams; the visual acuity, practical and any job-specific exams are given by your employer.

What's on the exam

ASNT NDT Level II UT
Review of Ultrasonic Techniques
6 key facts
Evaluation of Base Material Product Forms
6 key facts
Evaluation of Weldments
6 key facts
Evaluation of Bonded Structures
6 key facts
Discontinuity Detection
6 key facts
General Evaluation
6 key facts
Codes, Procedures and Specific Exam Application
6 key facts

Each branch is a topic in the official outline. Members see every key fact on the full mind map. Read the free study guide →

How to pass the ASNT NDT Level II UT exam

  • Check your exam date against 5 February 2027. Before it, the General exam follows six topics such as Evaluation of Weldments and Bonded Structures; after it, four domains covering principles and techniques, materials and product forms, data collection and reporting, and training, certification and safety.
  • The General exam allows 2.4 minutes per item. Know Snell's law, wavelength, near field, beam spread, decibels and skip geometry well enough to set each one up without hesitation on the ASNT calculator.
  • ASNT publishes no cut score for this exam. The 70% per exam and 80% composite figures often quoted come from employer programs under SNT-TC-1A, so treat 80% on each exam as your practice target.
  • After a failed exam you must reapply and wait 30 days. A passed Specific result stays valid for only 2 years if the General is not passed, so plan both exams close together.

Save your results and get your Readiness Score

Create a free account after the test: your score by topic, a mistakes bank, the complete study notes for the first topic, flashcards and the NDT Level III Formula Sheet.

Take the test first

What's in the premium ASNT NDT Level II UT prep

Premium ASNT NDT Level II UT prep is studied one topic at a time. Each step starts with that topic's key notes and flashcard deck, then its own question sets of 25, so you master one topic before you move to the next. When every topic is strong, the 6 full mock exams show you're ready.

3,000practice questions, every answer explained
6full-length mock exams, 50 questions each, timed
800flashcards with spaced repetition, sorted by topic
60comprehensive key notes across 7 topics

Your step-by-step study path

  1. 1
    Review of Ultrasonic Techniques9 key notes, 115 flashcards, then 450 practice questions in 18 sets of 25
    Notes free with an account
  2. 2
    Evaluation of Base Material Product Forms9 key notes, 115 flashcards, then 425 practice questions in 17 sets of 25
    Premium
  3. 3
    Evaluation of Weldments9 key notes, 115 flashcards, then 425 practice questions in 17 sets of 25
    Premium
  4. 4
    Evaluation of Bonded Structures9 key notes, 115 flashcards, then 425 practice questions in 17 sets of 25
    Premium
  5. 5
    Discontinuity Detection8 key notes, 115 flashcards, then 425 practice questions in 17 sets of 25
    Premium
  6. 6
    General Evaluation8 key notes, 115 flashcards, then 425 practice questions in 17 sets of 25
    Premium
  7. 7
    Codes, Procedures and Specific Exam Application8 key notes, 110 flashcards, then 425 practice questions in 17 sets of 25
    Premium
  8. Final step: 6 full mock exams50 questions each, timed like test day. Pass them, then book your exam.
    Premium
Free with an account

Read the complete ASNT NDT Level II UT study notes for “Review of Ultrasonic Techniques”

Our first full set of comprehensive notes, about 15 minutes of reading: Waves and velocity · Refraction and wave mode · Beam shape · Contact and immersion setups · Instruments and calibration, a worked exam example, the traps examiners use and a one-minute recap. Create a free account to read it and see how premium notes work before you decide.

Open the free dashboard

Study tools included

3,000 practice questions

3,000 exam-style questions per exam, organized topic by topic in sets of 25. Every answer explained, with the rule it comes from.

6 full mock exams

6 full-length timed mock exams per exam, with real question counts and time limits, so test day feels like practice day.

Exam Readiness Score

One 0 to 100 number that tells you when you're ready to book. Reach 80 and you're covered by our Pass Guarantee.

800 flashcards + spaced repetition

800 flashcards per exam, in a deck for each topic, that come back right before you'd forget them. Five minutes a day keeps every number fresh.

60 comprehensive key notes

60 key notes per exam, split across its topics and each explained in full: the concepts, worked exam examples, the traps examiners use and a quick recap. Your first set is free with an account.

Mind maps

See the whole exam on one screen: every topic and the facts under it.

Sample questions with answers

These are the questions in the free test above, with answers. Try the test first. You'll learn more by getting some wrong.

1. A shear-wave angle beam of 70 degrees is required in steel using an acrylic wedge. With acrylic longitudinal velocity 2,730 m/s and steel shear velocity 3,230 m/s, what wedge angle is needed?
Answer: 52.6°. Snell's law gives sin(wedge) = (2,730/3,230) x sin 70° = 0.794, so the wedge angle is about 52.6°. Using the steel longitudinal velocity instead gives about 25.7°, which would not produce the required shear refraction. Always match the velocity to the wave mode you want in the part.
2. A thickness gauge is left set to the velocity of steel (0.233 in/µs) and reads 1.000 in. on an aluminum plate with a velocity of 0.249 in/µs. What is the true thickness of the plate?
Answer: 1.069 in.. The gauge measures time, so true thickness equals the reading times the true velocity divided by the set velocity: 1.000 x 0.249/0.233 = 1.069 in. Dividing the other way gives 0.936 in. In a faster material a gauge set for a slower one reads thin.
3. A 2.25 MHz, 0.5 in. diameter straight-beam search unit is used on steel with a longitudinal velocity of 0.233 in/µs. What is the approximate beam spread half angle to the first null?
Answer: 14.6°. Wavelength is 0.233/2.25 = 0.104 in., and sin θ = 1.22 x 0.104/0.5 = 0.253, giving 14.6°. Leaving out the 1.22 constant gives 11.9°, and 29.3° is the full angle. A larger diameter or higher frequency narrows the beam.
4. A forged steel bar has grain flow along its length, and internal discontinuities are expected to lie along that flow. What is the primary beam direction for a straight-beam examination?
Answer: Radially, perpendicular to the grain flow. Discontinuities in forgings tend to elongate with grain flow, so sound must strike them broadside to return the strongest echo. An axial beam runs parallel to these flaws and reflects very little. A surface wave would only cover the surface and cannot reach the core.
5. A coarse-grained austenitic casting tested at 5 MHz shows heavy noise across the time base and a weak back wall. What change is most likely to improve the examination?
Answer: Lower the frequency to about 1 MHz. Coarse grains scatter short wavelengths strongly, so a lower frequency reduces scatter and restores penetration. A higher frequency makes the problem worse. Raising gain also raises the noise, so the signal-to-noise ratio does not improve.
6. A 45° angle-beam examination is done on a 1.00 in. thick plate. An indication peaks at a sound path of 2.00 in. Where is the reflector?
Answer: Depth 0.59 in., surface distance 1.41 in.. Surface distance is 2.00 x sin 45° = 1.41 in. The vertical travel is 2.00 x cos 45° = 1.41 in., which is more than one thickness, so the beam has bounced and the depth is 2 x 1.00 minus 1.41 = 0.59 in. Forgetting the bounce gives the 1.41 in. depth, which is impossible in a 1.00 in. plate.
7. A single-V weld has a 60° included angle (30° bevel on each side). Which shear-wave beam angle strikes the fusion face most nearly at normal incidence?
Answer: 60° shear wave. The fusion face sits 30° from the vertical, so its normal is 60° from the vertical, which matches a 60° beam. The 45° beam meets the face 15° off normal and returns a weaker echo from smooth planar lack of fusion. Angle selection matters most for flat, smooth reflectors.
8. On a single-V butt weld with a root bead, an angle-beam echo appears continuously along the weld. Plotted from each side, it falls at full thickness on the far side of the weld centerline. What is the most likely cause?
Answer: Root bead geometry, which is a nonrelevant reflector. A root bead reflects sound from beyond the centerline, and the same geometry shows from both sides, so continuous echoes plotted that way are usually geometric. A root crack or lack of root fusion would plot at the root on the near side of the centerline or at the centerline. Always plot the reflector before calling it.
9. A pulse-echo straight-beam test is applied to a thin aluminum skin adhesively bonded to a thick aluminum plate. Over a disbonded area, what change on the screen is most typical?
Answer: Skin reverberations strengthen and the far echo is lost. At a disbond, the air gap reflects almost all the sound back into the skin, so skin reverberations grow and little energy reaches the far surface. A good bond passes more sound through. The method cannot detect every weak bond, which is why reference standards are needed.
10. A straight-beam test changes from a 2.25 MHz to a 5 MHz search unit of the same diameter on fine-grained steel. Which outcome is expected?
Answer: Better flaw sensitivity but more attenuation. A higher frequency shortens the wavelength, improving sensitivity to small reflectors and resolution, but scatter and attenuation increase. It narrows the beam and lengthens the near field, so the reverse is wrong. Frequency is a trade-off between detail and penetration.
11. A corrosion survey must find thinning near the inside surface of a 0.150 in. wall pipe. A single-element contact straight-beam unit cannot separate close signals near the entry surface. Which change best helps?
Answer: Use a dual-element search unit focused near the area. A dual-element unit separates transmit and receive, removing the initial pulse from the display and improving near-surface resolution on thin walls. A lower frequency worsens resolution. Reject removes low-level signals and reduces linearity, so it should not be used to fix this.
12. A reference reflector is set to 80% FSH at 42 dB. A weld indication peaks at 40% FSH at 48 dB. How does the indication compare with the reference?
Answer: 12 dB below the reference. At 48 dB the indication reads 40% FSH, so at 42 dB it would read 20% FSH, and 20 log (20/80) is minus 12 dB. Ignoring the 6 dB gain difference gives minus 6 dB. Always bring both signals to the same gain before comparing amplitude.
13. During an angle-beam scan, an echo drops sharply when a couplant-wet finger is pressed on the surface between the search unit and the weld toe. What does this indicate?
Answer: A signal on or very near the scanning surface. A wet finger damps sound travelling along the surface, so an echo that responds is coming from the surface or just under it, such as a weld toe or surface wave. Reflectors deep in the weld do not change when the surface is touched. This quick test helps separate geometric signals from relevant ones.
14. On an AWS D1.1 ultrasonic examination, the instrument reads 44 dB at the indication level and 30 dB at the reference level. The sound path is 3.0 in. What is the indication rating?
Answer: +10 dB. The attenuation factor is 2 dB per inch of sound path beyond 1 in., so c = 2 x (3 - 1) = 4, and d = a - b - c = 44 - 30 - 4 = 10. Leaving out the attenuation factor gives 14, and forgetting to subtract the first inch gives 8. Rating is then read from the code acceptance table for thickness and angle.
15. Under ASME Section V Article 4, a contact examination is planned on a pipe with a 10 in. outside diameter. Which curved basic calibration block diameter is allowed, based on the 0.9 to 1.5 times rule?
Answer: 8 in.. An 8 in. block covers surfaces of 7.2 to 12 in. diameter, which includes the 10 in. pipe. A 12 in. block covers only 10.8 to 18 in., so the pipe is too small for it, while a 6 in. block stops at 9 in. Work out the range from the block diameter and not the other way around.

Get the full ASNT NDT Level II UT prep

Most popular · cancel anytime

Premium Monthly

$147/month
per exam
About $4.83 a day · less than a retake fee, for the certification that lets you approve procedures and certify technicians
  • One ASNT Level III exam of your choice: Basic, UT, RT or MT
  • 3,000 practice questions + 6 full mock exams per exam
  • 800 flashcards + 60 key notes per exam, by topic, plus mind maps
  • Spaced repetition + mistakes bank
  • Readiness Score & detailed reports
  • Video lessons as they release
  • Content updates during your access
  • 5 bonuses: NDT formula sheet, discontinuity atlas, study planner and more
  • Pass Guarantee: complete the prep, pass or 100% back

Renews monthly until you cancel. Cancel in two clicks from your account; you keep access until the end of the month you've paid for. No minimum term.

Best value · 3 months free

Premium Yearly

$1,323/year
per exam
Pay for 9 months, get 12. Save $441 against paying monthly.
  • One ASNT Level III exam of your choice: Basic, UT, RT or MT
  • 3,000 practice questions + 6 full mock exams per exam
  • 800 flashcards + 60 key notes per exam, by topic, plus mind maps
  • Spaced repetition + mistakes bank
  • Readiness Score & detailed reports
  • Video lessons as they release
  • Content updates during your access
  • 5 bonuses: NDT formula sheet, discontinuity atlas, study planner and more
  • Pass Guarantee: complete the prep, pass or 100% back

Renews once a year until you cancel. We email you before each renewal. Cancel any time from your account; you keep access until the end of the year you've paid for.

Pass Guarantee. Complete the full prep, sit your exam within 60 days, and if you don't pass we refund 100% of your subscription payments. See the requirements
Secure checkout by Stripe Card, Apple Pay, Google Pay Pass Guarantee

ASNT NDT Level II UT exam FAQ

How many questions are on the ASNT NDT Level II UT exam?

Two multiple-choice exams: General 50 items and Specific 40 items (general industry or pressure equipment sector), with a time limit of general 2 hours; specific 2 hours (4 hours in total). Format: computer-based multiple choice with a scientific calculator provided by asnt. asnt does not publish whether any reference is supplied during these exams; confirm with asnt. this prep covers only the written general and specific exams, not the employer's visual acuity, practical or job-specific exams.

What is the passing score for ASNT NDT Level II UT?

Not published by ASNT for this exam. ASNT says its criterion-referenced cut scores are typically 70% to 80%. Both the General and the Specific exam must be passed, so aim for 80% or higher on each in practice.

How much does the ASNT NDT Level II UT exam cost?

US$740 for ASNT members, US$820 for nonmembers (General plus one Specific exam). Retake of a failed exam or an added sector exam: US$370 / US$410. ASNT fees differ for members and nonmembers and can change, so confirm on the ASNT certification website before you apply.

Which languages is the ASNT NDT Level II UT exam offered in?

US English (ASNT offers an online NDT terminology dictionary in Korean, Mandarin, Spanish, UK English and Arabic).

Where do I take the ASNT NDT Level II UT exam?

Pearson VUE test centers and ASNT Authorized Exam Centers (in person, computer-based, no walk-ins).

Is this ASNT NDT Level II UT practice test free?

Yes. The 15-question practice test on this page is free, with an explanation for every answer and no signup. A free account also unlocks the complete study notes for the first topic. The full ASNT NDT Level II UT prep is Premium at $147 a month for this exam.

What's in the premium ASNT NDT Level II UT prep?

3,000 practice questions organized topic by topic (Review of Ultrasonic Techniques: 450; Evaluation of Base Material Product Forms: 425; Evaluation of Weldments: 425; Evaluation of Bonded Structures: 425; Discontinuity Detection: 425; General Evaluation: 425; Codes, Procedures and Specific Exam Application: 425), 6 full-length timed mock exams of 50 questions, 800 flashcards and 60 comprehensive key notes split across all 7 topics, plus a mistakes bank and the Readiness Score.

Related practice tests

Exam details are summarized from the official candidate information available in October 2026. ASNT changes formats and fees, so confirm with ASNT Certification Services LLC (American Society for Nondestructive Testing) before you book. NDTLevel3Exam is not affiliated with ASNT or Pearson VUE.

Start the free test